Title: | Otomotiv endüstrisinde kullanılan DD11 ve DD13 çelik levhaların robotik MAG kaynağında farklı kaynak parametrelerinin mikroyapı ve mekanik özelliklere etkisi | Other Titles: | The effects of different welding parameters on microstructure and mechanical properties in robotic MAG welding of DD11 and DD13 steel plates used in the automotive industry | Authors: | Tekbaş, Hasan Fatih | Advisors: | Onar, Volkan | Keywords: | DD11 DD13 MAG |
Publisher: | Pamukkale Üniversitesi Fen Bilimleri Enstitüsü | Abstract: | Bu çalışmada otomotiv endüstrisinde kullanımı yaygın olan DD11 ve DD13 düşük karbonlu çeliklerin robotik MAG kaynak yöntemi kullanılarak farklı kaynak parametrelerinde mikroyapı ve mekanik özellikleri incelenmiştir. Kaynaklı birleştirmelerde iki farklı gaz debisi kullanılmıştır. Gerçekleştirilen birleştirmelerde kaynak amperi olarak 240A, 250A ve 270A, kaynak hızı olarak da 12mm/sn ve 16mm/sn kullanılmıştır. Belirtilen parametreler kullanılarak DD11 ve DD13 levhalar birbirleri ile birleştirilmiştir. Kaynaklı birleştirmeler gerçekleştirildikten sonra her bir parametreden 3 adet olacak şekilde çekme numunesi kesilmiştir. Gerçekleştirilen çekme testleri neticesinde en yüksek çekme dayanımı 12mm/sn kaynak hızına ve 250A kaynak akımına sahip 10 numaralı numunede (326Mpa), en düşük çekme dayanımının ise 16mm/sn kaynak hızına ve 250A kaynak akımına sahip 3 numaralı numunede (241Mpa) olduğu saptanmıştır. Bu çalışma neticesinde DD11 ve DD13 plakaların optimum kaynak parametreleri tespit edilmiştir. In this study, microstructure and mechanical properties of DD11 and DD13 low carbon steels, which are widely used in the automotive industry, were investigated using robotic MAG welding method at different welding parameters.Two different gas flow rates are used in welded joints. 240A, 250A and 270A as welding amperes, 12mm/sec and 16mm/sec as welding speed were used in the joints performed. DD11 and DD13 boards were made, 3 tensile samples were cut from each parameter. As a result of the tensile test performed, it was determined that the highest tensile strength was found in sample 10 (326Mpa) with a welding speed of 12mm/sec and welding current of 250A, and the lowest tensile strength was found in sample Number 3 (241 Mpa) with a welding speed of 16mm/sec and a welding current of 250A. As a result of this study, optimum welding parameters of DD11 and DD13 plates were determined. |
URI: | https://hdl.handle.net/11499/45804 |
Appears in Collections: | Tez Koleksiyonu |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
Hasan Fatih Tekbaş.pdf | 4.47 MB | Adobe PDF | View/Open |
CORE Recommender
Page view(s)
332
checked on Aug 24, 2024
Download(s)
216
checked on Aug 24, 2024
Google ScholarTM
Check
Items in GCRIS Repository are protected by copyright, with all rights reserved, unless otherwise indicated.