Please use this identifier to cite or link to this item:
https://hdl.handle.net/11499/57993
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.advisor | Aksöz, Sinan | en_US |
dc.contributor.advisor | Pamuk, Özer | en_US |
dc.contributor.author | Duran, Hasan | en_US |
dc.date.accessioned | 2024-10-07T08:32:06Z | - |
dc.date.available | 2024-10-07T08:32:06Z | - |
dc.date.issued | 2024 | en_US |
dc.identifier.uri | https://hdl.handle.net/11499/57993 | - |
dc.description | Bu tez çalışması PAMUKKALE ÜNİVERSİTESİ BİLİMSEL ARAŞTIRMA PROJELERİ tarafından 2022FEBE052 nolu proje ile desteklenmiştir. | en_US |
dc.description.abstract | Bu çalışmada, ön alaşımlı 31CrMo12 çelik tozları kullanılarak toz metalurjisi (T/M) üretim yöntemi ile numune üretilmiştir. Numune üretim aşamasında, tozların preslenme sıcaklık değerleri ve basınç değerleri belirlenmiştir. Sinterleme aşamasında, preslenmiş tozlar, sinterleme ve borlama işlemlerinin eş zamanlı gerçekleştirildiği ve Boro-Sinterleme olarak adlandırılan yöntem kullanılarak hem borlama hem de sinterleme işlemleri tek seferde gerçekleştirilmiştir. Bu işlem, katı borlama kutusunda Ekabor2, Al2O3 ve SiC tozları ortamında uygulanmıştır. Boro-Sinterleme işlemi ile elde edilen numunelerin tribolojik davranışları incelenmiştir. Çalışmada kullanılan 31CrMo12 ön alaşımlı çelik tozları, atomizasyon yöntemiyle elde edilmiş olup, ortalama 20-30 μm boyut aralığında tozlardan oluşmaktadır. Tozlar, 200 MPa’da soğuk ve 600°C sıcaklıkta 300 MPa’da ılık olmak üzere iki aşamada preslenerek Boro-Sinterleme aşamasına geçilmiştir. Boro-Sinterleme işlemi, 950°C ve 1050°C’de 2, 4 ve 6 saat süresince gerçekleştirilmiştir. Boro-Sinterleme sonrasında üretilen numunelerin, Boro-Sinterleme sürecinin etkilerinin incelenebilmesi için yoğunlukları hesaplanmış, aşınma verileri oluşturulmuş ve mikro sertlik ölçümleri gerçekleştirilmiştir. Elde edilen veriler neticesinde numuneler arasındaki farklar ve değerler yorumlanmıştır. Boro-Sinterleme sonrasında numunelerin karakterizasyonu FESEM, EDS, OM ve XRD analizleriyle gerçekleştirilmiştir. Boro-Sinterleme sonucunda yüzeyde homojen yapılı borür tabakasının oluşumu sağlanmıştır. Boro-Sinterleme sonrasında numune sertliklerinde artış gözlemlenmiştir. Boro-Sinterleme sıcaklığı ve süresindeki optimizasyon ile numunelerin tribolojik davranışlarının iyileştiği gözlemlenmiştir. | en_US |
dc.description.abstract | In this study, samples were produced using pre-alloyed 31CrMo12 steel powders and the powder metallurgy (P/M) production method. During the sample production phase, the pressing temperature and pressure values of the powders were determined. In the sintering phase, the pressed powders were subjected to a simultaneous sintering and boronizing process, known as Boro-Sintering, where both processes were carried out in a single step. This process was performed in a solid boronizing box with Ekabor2, Al2O3, and SiC powders. The tribological behaviors of the samples obtained via the Boro-Sintering process were examined. The pre-alloyed 31CrMo12 steel powders used in the study were produced by the atomization method, with an average particle size range of 20-30 μm. The powders were pressed in two stages: cold pressing at 200 MPa and warm pressing at 300 MPa at 600°C, before moving on to the Boro-Sintering phase. The Boro-Sintering process was carried out at 950°C and 1050°C for durations of 2, 4, and 6 hours. After the Boro-Sintering process, the densities of the samples were calculated, wear data were compiled, and microhardness measurements were conducted to examine the effects of the Boro-Sintering process. Based on the obtained data, the differences and values between the samples were interpreted. The characterization of the samples after Boro-Sintering was conducted through FESEM, EDS, OM, and XRD analyses. As a result of the Boro-Sintering process, the formation of a homogeneous boride layer on the surface was achieved. An increase in the hardness of the samples was observed following the Boro-Sintering process. Optimization of the Boro-Sintering temperature and duration resulted in improvements in the tribological behaviors of the samples. | en_US |
dc.language.iso | tr | en_US |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.subject | Boro-Sinterleme | en_US |
dc.subject | Toz Metalurjisi | en_US |
dc.subject | 31CrMo12 | en_US |
dc.subject | triboloji | en_US |
dc.subject | Boro-Sintering | en_US |
dc.subject | Powder Metallurgy | en_US |
dc.subject | Tribology | en_US |
dc.title | 31CrMo12 ön alaşımlı T/M çeliklerde boro-sinterleme işlem parametrelerinin belirlenerek tribolojik davranışlarının incelenmesi | en_US |
dc.title.alternative | Determination of boro-sintering process parameters and investigation of tribological behaviors in 31CrMo12 pre-alloyed T/M steels | en_US |
dc.type | Master Thesis | en_US |
dc.department | PAÜ, Enstitüler, Fen Bilimleri Enstitüsü | en_US |
dc.relation.publicationcategory | Tez | en_US |
dc.contributor.affiliation | Pamukkale Üniversitesi | en_US |
item.openairetype | Master Thesis | - |
item.openairecristype | http://purl.org/coar/resource_type/c_18cf | - |
item.cerifentitytype | Publications | - |
item.fulltext | With Fulltext | - |
item.languageiso639-1 | tr | - |
item.grantfulltext | open | - |
Appears in Collections: | Tez Koleksiyonu |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
Hasan Duran YL TEZ son 1 17.09.2024.pdf | 8.05 MB | Adobe PDF | View/Open |
CORE Recommender
Items in GCRIS Repository are protected by copyright, with all rights reserved, unless otherwise indicated.